Because of the glues and mixed species nature of these materials, it is very difficult to take reliable readings with pin-type or Wagner Meters Handheld Moisture Meters.

Note: However, if you would like to work up your own meter calibrations for materials you use repetitively, you can contact Wagner Meters for guidelines and suggestions.